Screed is the levelling and load-transfer layer between the structural concrete slab and the final floor finish. Its job is not decorative: it sets the level, spreads the load and leaves a smooth surface for the finish to bond to. A large share of the flooring complaints we see on site stem not from the finish but from the screed beneath it.

What exactly does screed do?

The top of a slab never comes out level enough to lay a finish on. Screed does three jobs at once: it brings the surface to level, embeds and protects service pipes, and spreads the load from the finish to the base. Where there is thermal insulation or underfloor heating, screed is also the layer that distributes the heat.

  • Level and fall: in wet rooms, the fall towards the drain is set with the screed.
  • Pipe protection: if not enough screed is left over a pipe, that run cracks in the first year.
  • Load distribution: point loads are spread over a wide area, so the finish does not crack.

Types of screed: which one where?

Three families are most common in practice.

  • Bonded screed. Applied directly to the concrete slab. It is the type that can be laid thinnest; the surface must be clean and the bond strong. Screed bonded to dusty or uncured concrete lifts off in sheets within a few months.
  • Unbonded screed. A separating layer (polythene, membrane) goes in between. It acts independently of the structure; preferred where there is a risk of moisture from below, and laid thicker.
  • Floating screed. Laid over an insulation board. It is the standard for underfloor-heated floors and floors requiring acoustic insulation; it always needs an edge strip at the perimeter.

By binder, alongside the conventional cement-based screed there are fast-drying anhydrite (calcium sulphate) based and self-levelling screed types. Self-levelling products are for thin levelling; where thickness is required, conventional screed is the economical choice.

Thickness and level: the most common mistake

Screed thickness is chosen not at will but according to its type and the layer beneath it. Bonded screed can stay thin; unbonded and floating screeds must be thicker to carry the load on them without cracking. In underfloor heating, the thickness left over the pipe is a separate matter — thin screed touching the pipe cracks in the first heating season.

Level errors, on the other hand, start at the shell stage. If the finish thickness (tile + adhesive, parquet + underlay) is not accounted for from the outset, door frames and threshold levels will not line up. The finished floor level should be marked in every room before the screed is laid.

Why does screed crack?

There is no single cause of cracking, but the list is short:

  • Too much water. Water added to the mix to make it easier to lay means shrinkage as it dries. Adjust consistency with the right mix, not with water.
  • No curing. Wind and sun dry the surface before the interior; the surface shrinks, the bottom holds, and a crack forms. Bodrum’s summer wind does not forgive this mistake.
  • No joints. If expansion and separation joints are not left in large areas, the screed chooses where to crack by itself.
  • Forgetting the edge strip. A floating screed bonded to the wall has nowhere to expand.

Pre-flooring checklist

  1. Has the surface moisture been measured? Parquet glued to a damp screed lifts.
  2. Have level and fall been checked? With a spirit level and straightedge, room by room.
  3. Is the surface dusty or loose? Apply a primer if necessary.
  4. Have the joints been carried through into the finish?
  5. Are there hollow (drum-sounding) areas? Check by tapping with a mallet.

Screed is the most expensive layer to correct afterwards: once tiles are laid on top, a fault is fixed by ripping up. An hour of checking on the day of laying is cheaper than a week of removal.

Frequently Asked Questions

How many days does screed take to dry, and when can the finish go on?
Being walkable and being ready for a finish are two different things. Cement-based screed hardens at the surface within a few days, but the waiting time before the finish depends on thickness, air temperature and ventilation. The decision should be made by moisture measurement, not by the calendar.
Is insulation under the screed essential?
Yes, in ground-bearing slabs and underfloor heating systems. Uninsulated screed loses heat to the ground; and in upper-floor slabs, impact sound insulation is again provided by this layer.
Should cracked screed be removed?
It depends on the type of crack. Superficial shrinkage cracks can usually be closed with a suitable repair mortar and primer. If the screed has separated from the structure (sounds hollow), that area is removed and redone; covering it over does nothing but postpone the problem.
When is the screed heated in an underfloor-heated floor?
The first heating is done after the screed has set sufficiently, and gradually. Switching the system straight to a high temperature means sudden expansion and cracking in the screed; the heat-up programme is staged according to the manufacturer’s instructions.